J Mech Behav Biomed Mater ; 154: 106533, 2024 Jun.
Article in English | MEDLINE | ID: mdl-38598918

ABSTRACT

The present work aims to develop a production method of pre-sintered zirconia-toughened-alumina (ZTA) composite blocks for machining in a computer-aided design and computer-aided manufacturing (CAD-CAM) system. The ZTA composite comprised of 80% Al2O3 and 20% ZrO2 was synthesized, uniaxially and isostatically pressed to generate machinable CAD-CAM blocks. Fourteen green-body blocks were prepared and pre-sintered at 1000 °C. After cooling and holder gluing, a stereolithography (STL) file was designed and uploaded to manufacture disk-shaped specimens projected to comply with ISO 6872:2015. Seventy specimens were produced through machining of the blocks, samples were sintered at 1600 °C and two-sided polished. Half of the samples were subjected to accelerated autoclave hydrothermal aging (20h at 134 °C and 2.2 bar). Immediate and aged samples were characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD). Optical and mechanical properties were assessed by reflectance tests and by biaxial flexural strength test, Vickers indentation and fracture toughness, respectively. Samples produced by machining presented high density and smooth surfaces at SEM evaluation with few microstructural defects. XRD evaluation depicted characteristic peaks of alpha alumina and tetragonal zirconia and autoclave aging had no effect on the crystalline spectra of the composite. Optical and mechanical evaluations demonstrated a high masking ability for the composite and a characteristic strength of 464 MPa and Weibull modulus of 17, with no significant alterations after aging. The milled composite exhibited a hardness of 17.61 GPa and fracture toughness of 5.63 MPa m1/2, which remained unaltered after aging. The synthesis of ZTA blocks for CAD-CAM was successful and allowed for the milling of disk-shaped specimens using the grinding method of the CAD-CAM system. ZTA composite properties were unaffected by hydrothermal autoclave aging and present a promising alternative for the manufacture of infrastructures of fixed dental prostheses.


Subject(s)
Aluminum Oxide , Ceramics , Materials Testing , Aluminum Oxide/chemistry , Ceramics/chemistry , Surface Properties , Zirconium/chemistry , Computer-Aided Design , Dental Materials
2.
Clin Exp Dent Res ; 10(2): e869, 2024 04.
Article in English | MEDLINE | ID: mdl-38433287

ABSTRACT

OBJECTIVE: This study aimed to compare the color change of computer-aided design (CAD)/computer-aided manufacturing (CAM) polymethyl methacrylate (PMMA) denture teeth and conventional acrylic teeth after immersion in three staining beverages (coffee, red tea, and cola) for a day, 7 days, and 30 days. MATERIALS AND METHODS: Group 1: Conventional acrylic teeth (n = 32). Group 2: Milled CAD/CAM teeth out of PMMA disc (n = 32). The specimens of each material were further divided into four subgroups: (1) Control group, distilled water (n = 16). (2) Red tea solution (n = 16). (3) Coffee solution (n = 16). (4) Cola (n = 16). The color change ( ∆ E $\unicode{x02206}E$ ) was assessed using a spectrophotometer at four time points: at the baseline (t0 ), on the 1st day (t1 ), on the 7th day (t2 ), and the 30th day (t3 ) of immersion. Kolmogorov-Smirnov test was applied, followed by performing independent samples t test, one-way analysis of variance and post-hoc Tukey tests to compare the color change values at different time points. RESULTS: The mean score of NBS values of the coffee solution indicates perceivable color change at the end of the 30th day in the conventional acrylic teeth group. It was 0.843 ± 0.395 at t1 , then increased to 1.017 ± 0.477 at t2 and to 2.259 ± 1.059 at t3 . There is a statistically significant difference (p < 0.05) in color change values between both tooth types at the end of the 30th day of immersion in red tea solution and a statistically significant difference at the end of the 7th day (p < 0.05) and the 30th day (p < 0.05) of immersion in coffee solution. CONCLUSIONS: CAD/CAM PMMA teeth are more color stable than conventional acrylic teeth after 30 days of immersion in coffee and red tea solution.


Subject(s)
Coffee , Polymethyl Methacrylate , Beverages , Computer-Aided Design , Staining and Labeling , Dentures , Tea
3.
J Esthet Restor Dent ; 36(3): 477-483, 2024 Mar.
Article in English | MEDLINE | ID: mdl-37877244

ABSTRACT

OBJECTIVE: The purpose of this in vitro study was to evaluate the effect of potassium aluminum sulfate (alum) application on the stainability and translucency of computer-aided design and computer-aided manufacturing (CAD-CAM) materials after coffee thermocycling (CTC). MATERIALS AND METHODS: Disk-shaped specimens (Ø10 × 1 mm; N = 200) were fabricated by using additively (Crowntec [CT] and Varseo Smile Crown Plus [VS]) and subtractively manufactured (Brilliant Crios [RCR], CEREC Block [FC], and Vita Enamic [VE]) CAD-CAM materials and polished. All specimens were randomly divided into two groups as alum applied and control (n = 10). All specimens were then subjected to CTC (10,000 cycles at 5-55°C) and color coordinates were measured at each time interval. Color differences (ΔE00 ) and relative translucency parameters (RTPs) were calculated and the data were statistically analyzed (a = 0.05). RESULTS: Among tested time intervals, alum applied specimens had their lowest ΔE00 after alum application (p ≤ 0.006), except for FC (p = 0.177). In addition, alum applied RCR had lower ΔE00 values than its control specimens (p = 0.029). Alum applied specimens had their lowest RTP after CTC (p < 0.001) and alum application decreased the RTP of CT (p = 0.010). CTC reduced the RTP of all materials in control groups (p < 0.001). Alum applied CT had higher RTP than its control specimens (p = 0.049). CONCLUSIONS: Alum application's effect on color change varied depending on the material and alum mostly resulted in clinically acceptable changes in translucency. CTC led to unacceptable color and translucency changes based on previously reported threshold values. CLINICAL SIGNIFICANCE: Optical properties of CAD-CAM materials and the sustainability of these properties over time is critical for longevity. Alum may improve the color stability of reinforced composite resin when subjected to long-term coffee consumption.


Subject(s)
Alum Compounds , Coffee , Dental Porcelain , Color , Materials Testing , Surface Properties , Ceramics , Computer-Aided Design
4.
Am J Dent ; 36(6): 310-316, 2023 12.
Article in English | MEDLINE | ID: mdl-38092749

ABSTRACT

PURPOSE: To examine the effects of coffee staining and bleaching applications on the optical properties of CAD-CAM blocks, and to provide a three-dimensional visualization of surface changes with atomic force microscope (AFM). METHODS: 80 samples were prepared from four different CAD-CAM blocks: [Cerec (CR), Shofu (SH), Cerasmart (CRS), Lava Ultimate (LU)], and a microhybrid composite resin [Filtek Z250 (Z250)]. After staining, the samples were divided into two subgroups according to bleaching methods: 16% carbamide peroxide (HB), and 40% hydrogen peroxide (OB). Color measurements were performed at baseline (t0), after staining (t1), and after bleaching (t2) to obtain translucency parameters (TP00), color change (ΔE00), and whiteness index (WID) values. Surface roughness analysis (Ra) was performed with AFM after coffee staining and bleaching procedures (at t1 and t2). Data were analyzed with Generalized Linear Model, and Bonferroni correction (P< 0.05). RESULTS: TP00 values increased only in the CRS group after the bleaching application, and the effect of method was again observed only in CRS. While bleaching increased WID values of all groups except CRS, no difference was found between bleaching methods. Regardless of evaluation time, the roughest group is Z250, and the only difference between bleaching methods was observed in the CR group. In conclusion, the effects of staining and bleaching applications on the optical and surface properties of CAD-CAM blocks are material-dependent. CLINICAL SIGNIFICANCE: Effective bleaching of discolored CAD-CAM materials was achieved regardless of the bleaching method used, and without any significant adverse effect on the surface properties of the materials.


Subject(s)
Coffee , Composite Resins , Materials Testing , Color , Ceramics , Staining and Labeling , Surface Properties , Computer-Aided Design
5.
Int J Prosthodont ; 36(6): 120-132, 2023 Dec 18.
Article in English | MEDLINE | ID: mdl-38112735

ABSTRACT

PURPOSE: To evaluate and compare the effect of accelerated aging and coffee immersion on the microhardness and gloss of a new computer-aided design and computer-aided manufacturing (CAD/CAM) hybrid material (Crystal Ultra) to those of contemporary restorative materials. MATERIALS AND METHODS: A total of 160 specimens (12 × 14 × 1 mm ± 0.05 mm) were obtained from IPS e.max (IPS), VITA Enamic (VE), Crystal Ultra (CU), Lava Ultimate (LU), and CeraSmart (CS) high-translucency CAD/CAM blocks. The Vickers microhardness and gloss of the specimens were determined after thermocycling and coffee immersion. Data analysis was performed using SPSS (α = .05). RESULTS: IPS and CS specimens exhibited the highest (572.66 ± 11.30) and lowest (61.92 ± 3.91) microhardness, respectively. The highest gloss was observed with IPS specimens (3.31 ± 0.32), and LU specimens showed the lowest gloss (2.33 ± 0.06). A significant difference in gloss was observed between the materials at all measurement intervals (P < .01), except at T0 (P = .43). IPS specimens showed no significant changes in either group at any measurement interval. CONCLUSIONS: The microhardness and gloss of the new CU material were comparable to those of the tested contemporary hybrid restorative materials. Glass-ceramic showed superior hardness and gloss compared to hybrid restorative materials. Accelerated aging with thermocycling and staining significantly affected the microhardness and gloss of all tested CAD/CAM materials.


Subject(s)
Coffee , Dental Porcelain , Dental Porcelain/chemistry , Immersion , Materials Testing , Ceramics , Dental Materials/chemistry , Computer-Aided Design , Surface Properties
6.
Gen Dent ; 71(6): 24-30, 2023.
Article in English | MEDLINE | ID: mdl-37889241

ABSTRACT

The esthetic outcome of temporary prostheses, especially those in the anterior area, is of primary importance. The purpose of this in vitro study was therefore to evaluate the color stability of 3 temporary restorative materials: self-curing (SC) acrylic resin (Tempron); heat-curing acrylic resin (SR Ivocron); and polymethyl methacrylate resin blocks (Telio CAD) machined using computer-aided design/computer-aided manufacturing (CAD/CAM) technology. The heat-curing material was polymerized with either a pressure-curing technique (PT) or a flasking technique (FT). As a result, there were 4 experimental groups: SC, PT, FT, and CAD/CAM. Sixteen specimens were prepared for each group. After polymerization or milling, all specimens were polished using a diamond polishing paste, and 1 specimen from each group was exposed to Fourier-transform infrared (FTIR) and ultraviolet visible (UV-Vis) spectroscopy before immersion. The specimens were exposed to pigmented beverage agents (coffee, cola, turmeric solution, or tea), and the color change was monitored for 4 weeks using FTIR and UV-Vis spectroscopy as well as by macroscopic observation of the specimens (n = 4 per group per immersion period). The PT specimens showed the most significant color change, followed by the SC specimens. A less significant color variation was noted in the FT specimens, and insignificant change was reported in the CAD/CAM group. The solution that had the most significant staining effect was turmeric, and the CAD/CAM resin showed the greatest color stability of the tested materials. Color stability depends on the material used, the polymerization technique, the polishing steps, the pigmentation agent, and the duration of exposure to the agent.


Subject(s)
Dental Implants , Humans , Beverages , Acrylic Resins , Coffee/chemistry , Polymethyl Methacrylate , Computer-Aided Design , Materials Testing , Surface Properties , Color , Dental Materials/chemistry
7.
J Mech Behav Biomed Mater ; 148: 106192, 2023 12.
Article in English | MEDLINE | ID: mdl-37865017

ABSTRACT

The aim of this in vitro study was to evaluate the surface roughness, translucency, fatigue failure load (FFL), and number of cycles for fatigue failure (CFF) of a recently released lithia-based material called advanced lithium disilicate and three other ceramics indicated for monolithic restorations. First, ALD (advanced lithium disilicate, CEREC Tessera, Dentsply Sirona), LD (lithium disilicate, IPS e. max CAD, Ivoclar), LS (lithium silicate-disilicate, Suprinity, Vita Zahnfabrik), and 4Y-PSZ (Yttria-stabilized zirconia, IPS e.max ZirCAD MT, Ivoclar) discs (n = 15, Ø = 10 mm and thickness = 1.0 mm) were fabricated from CAD/CAM blocks/discs, A2 shade. The discs were sintered/crystallized and subsequently analyzed by a rugosimeter (Mitutoyo SJ-410) to determine Ra and Rz surface roughness parameters. Next, they were evaluated to determine the translucency parameter (TP) using a bench-top spectrophotometer (SP60, EX-Rite). The discs were subsequently cemented to glass fiber epoxy resin discs, and the specimens were tested under cyclic loading (Step-test), immersed in distilled water at a frequency of 20 Hz, with an initial cyclic load of 200 N for 5,000 cycles and increments of 50 N every 10,000 cycles until failure. Fatigue failure load (FFL) and number of cycles for fatigue failure (CFF) were recorded for subsequent Kaplan Meier analysis, with post-hoc Mantel-Cox and Weibull analysis (α = 0.05). Complementary fractographic, topographic and energy dispersive spectroscopy analyses (EDS) were performed. 4Y-PSZ showed higher survival (p < 0.05), with higher FFL and CFF (1077 N; 180,333 cycles), followed by LD (980 N; 161,000 cycles), LS (937 N; 152,333 cycles) and ALD (910 N; 147,000 cycles). No differences were observed between the tested groups regarding Weibull modulus. ALD presented TP (28.14) equal to DL (28.27) and higher than LS (25.51). All lithia-based materials had higher translucency than 4Y-PSZ (TP = 8.62) (p < 0.05). ALD appears to have a similar elemental composition to LD and LSD for oxygen and silicon. ALD and LSD have a similar zirconium content. Fractures originated on the cemented surface of the ceramic discs. Lithia-based ceramics showed lower surface roughness, with ALD (Ra = 0.04 µm; Rz = 0.66 µm) showing the lowest values (p < 0.05). Despite showing lower FFL when compared to LD and 4Y-PSZ, ALD has compatible translucency and mechanical fatigue performance with its indication for fabricating monolithic, anterior and posterior adhesively cemented single-unit restorations. However, further studies are needed to substantiate its clinical performance.


Subject(s)
Ceramics , Dental Porcelain , Ceramics/chemistry , Surface Properties , Materials Testing , Dental Stress Analysis , Zirconium/chemistry , Computer-Aided Design
8.
Am J Dent ; 36(5): 227-232, 2023 Oct.
Article in English | MEDLINE | ID: mdl-37865809

ABSTRACT

PURPOSE: To evaluate staining- and aging-dependent changes in the color and translucency of 3D-printed resin-modified ceramics (RMC). METHODS: Specimens (n= 5 per condition and material) were fabricated from test materials: Permanent Crown Resin (PCR), Crowntec (CT), Vita Enamic (VE) and Tetric CAD (TC). Specimens were stained in wine, coffee, tea, and water (control) and exposed to artificial accelerated aging (AAA). Color measurements were obtained using a spectrophotometer at baseline (T0) and at 3.5 (T1) and 7 (T2) days after immersion. For AAA, measurements were obtained at baseline (T0) and after exposure to controlled irradiance of 150 kJ/m² (T1) and 300 kJ/m² (T2). Mean and standard deviations were calculated on CIEDE2000 color differences (ΔE00), translucency parameter (TP00) and treatment-dependent changes in the translucency parameter (ΔTP0 0). Differences between materials and test conditions were tested by one-way ANOVA (α= 0.05). Results were additionally interpreted using visual color difference thresholds in dentistry ΔE00= 0.8 for the 50:50 perceptibility threshold (PT) and ΔE00= 1.8 for the 50:50 acceptability threshold (AT). ΔTP00 values were interpreted using 5058;50 TPT00= 0.6 and 50:0% TAT00= 2.6. RESULTS: Statistically significant differences were found among the materials when exposed to the different test conditions. At the T0-T1 time interval, the highest color difference was found with wine (0.1-2.2) on all materials except CT, which showed the highest ΔE00 with AAA (2.5). The second highest color differences were obtained upon exposure to AAA (0.2-2.5) and tea (0.5-1.1). The TP00 at baseline ranged from 5.1 to 9.8. Significant differences in ΔTP00 were found among the tested materials and staining/aging conditions, but no significant differences were found among the staining/aging intervals (T0-T1, T0-T2 and T1-T2). CLINICAL SIGNIFICANCE: Staining- and artificial aging-dependent changes of 3D-printed and milled resin modified ceramics used for definitive restorations could represent a challenge in terms of restoration acceptability or dissatisfaction. Staining and aging conditions produced significant color changes, while translucency changes were not significant.


Subject(s)
Ceramics , Tea , Color , Materials Testing , Staining and Labeling , Surface Properties , Printing, Three-Dimensional , Computer-Aided Design
9.
Oper Dent ; 48(5): 588-598, 2023 Sep 01.
Article in English | MEDLINE | ID: mdl-37635458

ABSTRACT

OBJECTIVE: This study aimed to investigate the surface roughness, microhardness, and color changes of resin-based computer-aided design/computer-aided manufacturing (CAD/CAM) blocks and 3D-printed permanent resins in different beverages. METHODS AND MATERIALS: Resin-based CAD/CAM blocks (Cerasmart 270 and Grandio Blocs) and 3D-printed permanent restorative resins (Crowntec and Permanent Crown) were used in this study. A total of 96 specimens were prepared from CAD/CAM blocks and 3D-printed permanent resins. The initial surface roughness, microhardness, and shade value of the specimens were measured. Then, the specimens prepared from each material were divided into three subgroups (n=8) and immersed in tea, coffee, and distilled water for 30 days. After the specimens were immersed in the beverages, the surface roughness, microhardness, and tone values were measured again. The data were statistically analyzed using a two-way analysis of variance test (p<0.05). RESULTS: No statistically significant difference was found in the surface roughness values of the resin-based CAD/CAM blocks and 3D-printed resins (p<0.05). Resin-based CAD/CAM blocks showed statistically significantly higher microhardness than 3D-printed permanent resins (p<0.05). Although the color changes in 3D-printed resins in tea and coffee were similar to those in resin-based CAD/CAM blocks on the first and seventh days, more color changes appeared in the 3D-printed resins after 30 days. The surface roughness and microhardness values of the specimens submerged in tea, coffee, and distilled water showed no statistically significant changes (p<0.05). CONCLUSIONS: Although the surface roughness of 3D-printed permanent resins was similar to that of resin-based CAD/CAM blocks, they had a lower microhardness value. Moreover, 3D-printed permanent resins showed more color changes in tea and coffee.


Subject(s)
Coffee , Computer-Aided Design , Surface Properties , Printing, Three-Dimensional , Water , Tea
10.
J AOAC Int ; 106(6): 1608-1619, 2023 Nov 02.
Article in English | MEDLINE | ID: mdl-37449906

ABSTRACT

BACKGROUND: Solid phase extraction (SPE) techniques, based on computationally designed magnetic-based multi-targeting molecular imprinted polymer (MT-MIP), combined with UV spectrophotometric approaches provide advantages in the examination of counterfeit samples. OBJECTIVE: The current work describes an innovative and sustainable methodology for the simultaneous determination of tadalafil (TAD) and dapoxetine hydrochloride (DAP) in aphrodisiac counterfeit products (honey and instant coffee) utilizing SPE exploiting MT-MIP. Additionally, an innovative UV spectrophotometric method capable of resolving TAD in its pharmaceutical binary mixtures with DAP was developed. A novel computational approach was implemented to tailor the synthesis and design of the MT-MIP particles. METHODS: We applied a newly developed UV spectrophotometric method which was based on a Fourier self-deconvolution (FSD) method coupled with the isoabsorptive point for determination of TAD and DAP in pharmaceutical dosage form. We also applied an SPE process based on MT-MIP designed particles, assisting in the analysis of both drugs in counterfeit food samples. The SPE process and the UV spectroscopic methodology were assessed regarding their greenness using the pioneering green analytical procedure index (GAPI), analytical greeness including sample preparation (AGREEprep) and AGREE tools. The synthesized MT-MIP particles were characterized by scanning electron microscopy and energy-dispersive x-ray spectroscopy. RESULTS: The suggested spectrophotometric methods revealed a wide linear concentration range of 2-50 µg/mL with lower LODs in the range of 0.604-0.994 µg/mL. Additionally, the suggested method demonstrated the utmost sensitivity and eco-friendliness for their target in its mixed dosage form and counterfeit food products. CONCLUSION: The SPE process and the developed analytical UV spectroscopic methodology were validated as per the ICH guidelines, and were found to be suitable for overseeing some counterfeiting activities in commercially available honey and instant coffee aphrodisiac products. HIGHLIGHTS: An SPE method based on MT-MIP magnetic-based polymer and a UV spectroscopic method were successfully developed for analysis of TAD and DAP in different matrices.


Subject(s)
Aphrodisiacs , Molecular Imprinting , Polymers/chemistry , Molecular Imprinting/methods , Coffee , Solid Phase Extraction/methods , Computer-Aided Design , Pharmaceutical Preparations , Magnetic Phenomena
11.
Med Sci Monit ; 29: e939341, 2023 Feb 07.
Article in English | MEDLINE | ID: mdl-36747464

ABSTRACT

BACKGROUND The majority of dental professionals currently recognize lithium disilicate E-max ceramic veneers as a the most widely used, conservative, and effective cosmetic materials in dentistry. This study aimed to compare the degree of surface changes - roughness (Ra), depth (Rz), and mean color changes (ΔE00) - of computer-aided design-computer-aided manufactured (CAD/CAM) ceramic veneers materials of varying thicknesses caused by staining by green tea, coffee, and Coca-Cola using digital spectrophotometer. MATERIAL AND METHODS This study was conducted at King Khalid University, College of Dentistry. Lithium disilicate glass ceramic (LDGC) material was used to create 60 rectangular slices using the CAD/CAM system. The material thickness and the type of beverage were measured. The specimens were immersed in beverages according to the manufacturer's instructions. Specimen description and tomography were completed with a 3D noncontact surface metrology using interferometry. The "VITA Easy-Shade" spectrophotometer was used to measure ΔE00. It was recorded after 2 weeks for different material thicknesses after immersing samples in green tea, coffee, and Coca-Cola staining materials.f RESULTS Significant changes in ceramic thickness were found in Ra and Rz of 0.07 and 1.00 mm after 14 days of staining. Coca-Cola showed a significant difference in Ra and Rz with 1.00 mm thickness measurement compared to the 0.07 mm group with ≤ of 0.05, which was considered statistically significant. Highest ΔE00 were recorded among samples stained by Coca-Cola, followed by coffee, for both thicknesses. CONCLUSIONS Those findings support previous studies using spectrophotometric analysis of staining of CAD-CAM ceramic veneers that Coca-Cola followed by coffee resulted in the greatest color ΔE00 change.


Subject(s)
Coca , Humans , Coffee , Tea , Cola , Color , Materials Testing , Ceramics , Dental Porcelain , Computer-Aided Design , Carbonated Beverages , Computers , Surface Properties
12.
J Prosthet Dent ; 129(3): 507.e1-507.e6, 2023 Mar.
Article in English | MEDLINE | ID: mdl-36737355

ABSTRACT

STATEMENT OF PROBLEM: A nanographene-reinforced polymethyl methacrylate (PMMA) has been introduced for definitive prostheses. However, knowledge on the surface roughness and stainability of this material is lacking. PURPOSE: The purpose of this in vitro study was to compare the surface roughness and stainability of nanographene-reinforced PMMA with those of a prepolymerized PMMA and a reinforced composite resin after coffee thermocycling. MATERIAL AND METHODS: Disk-shaped specimens (Ø10×1.5-mm) were prepared from 3 different A1-shade millable resins (prepolymerized PMMA [M-PM; PMMA]; nanographene-reinforced PMMA [G-CAM; G-PMMA]; reinforced composite resin [Brilliant Crios; RCR]). Surface roughness (Ra) values were measured before and after conventional polishing by using a noncontact profilometer. Initial color coordinates were measured over a gray background with a spectrophotometer after polishing. Specimens were then thermocycled in coffee for 5000 cycles. Measurements were repeated after coffee thermocycling, and color differences (ΔE00) were calculated. Ra values among different time intervals were analyzed by using either the Friedman and Dunn tests (RCR) or repeated measures analysis of variance (ANOVA) and Bonferroni corrected paired samples t tests (PMMA and G-PMMA), while Ra values within a time interval were analyzed by using either the Kruskal-Wallis and Dunn tests (before polishing) or 1-way ANOVA and Tukey HSD (after polishing) or Tamhane T2 tests (after coffee thermocycling). ΔE00 values were analyzed by using 1-way ANOVA and Tukey HSD tests, while color coordinates of the specimens after polishing and after coffee thermocycling were compared by using paired samples t tests (α=.05). RESULTS: All materials had their highest Ra values before polishing (P≤.011), while differences after polishing and after coffee thermocycling values were nonsignificant (P≥.140). PMMA had higher Ra than RCR before polishing (P=.002), and RCR had higher values than G-PMMA after polishing and after coffee thermocycling (P≤.023). RCR had the highest ΔE00 (P<.001). Polishing increased the b∗ values of PMMA, and coffee thermocycling increased the a∗ values of G-PMMA and all values of RCR (P≤.012). CONCLUSIONS: The tested materials had similar and acceptable surface roughness after polishing. The surface roughness of materials was not affected by coffee thermocycling. Considering the reported color thresholds, all materials had acceptable color change, but the computer-aided design and computer-aided manufacturing composite resin had perceptible color change after coffee thermocycling.


Subject(s)
Coffee , Dental Implants , Polymethyl Methacrylate , Materials Testing , Surface Properties , Color , Composite Resins , Computer-Aided Design
13.
J Dent ; 130: 104423, 2023 03.
Article in English | MEDLINE | ID: mdl-36642325

ABSTRACT

OBJECTIVES: To assess the effect of aging procedures on color, gloss and surface roughness of CAD/CAM composite materials. METHODS: 6 CAD/CAM composite materials (Brilliant CRIOS, Cerasmart, Lava Ultimate, Tetric CAD, Shofu Block HC, Grandio Blocs) were tested. 10 CAD/CAM fabricated specimens of each material polished according to manufacturers' recommendations, were subjected to one of the following aging procedures; immersion in coffee (30 days, 37οC), water thermocycling (5000 cycles, 5-55 °C) and photoaging (150,000 kJ/m2). Color, gloss and surface roughness measurements were performed before and after aging and the respective changes were calculated. Kruskal-Wallis tests, paired t-tests, one-way ANOVA and Bonferroni post-hoc tests were used for statistical analysis (a = 0.05). RESULTS: Color changes ranged from 3.03 to 4.13 after coffee immersion, from 1.33 to 2.55 after thermocycling and from 1.02 to 2.75 after photoaging. No statistically significant differences for ΔE*ab were found among materials after coffee immersion and thermocycling (p>0.05). Gloss changes ranged from -5.7 to -1.6 GU after coffee immersion, from -2.3 to 0.1 GU after thermocycling and from -4.4 to 0.5 GU after photoaging. No significant differences in gloss changes were found among materials after aging (p>0.05). Tetric CAD demonstrated the significantly lower gloss and the higher surface roughness after polishing. Except for gloss after thermocycling, aging procedures caused significant alteration of gloss and surface roughness parameters from baseline levels. CONCLUSIONS: Aging procedures caused perceptible but acceptable color changes and small but visible gloss changes, while surface roughness parameters of the tested CAD/CAM composite materials were significantly affected by aging. CLINICAL SIGNIFICANCE: Aging procedures affected CAD/CAM composite materials indicating that these materials may be prone to color and surface alterations in the oral environment that could compromise the esthetics and the performance of the restorations. Clinical studies are needed to investigate the long-term behavior of the newly introduced CAD/CAM materials.


Subject(s)
Ceramics , Coffee , Materials Testing , Surface Properties , Esthetics, Dental , Composite Resins , Computer-Aided Design , Color
14.
Dent Mater J ; 42(1): 64-71, 2023 Jan 31.
Article in English | MEDLINE | ID: mdl-36244740

ABSTRACT

The purpose of this study was to clarify the discoloration of fiber-reinforced composite resin (FRC) disc materials. The color differences (ΔEs) of three CAD/CAM disc materials, FRC with different fiber orientations, composite resin, and polyether-ether-ketones were evaluated after month-long immersion in water, coffee, and curry. The ΔEs of all materials after coffee and curry immersion increased with increasing immersion periods, while those after water immersion barely increased. FRC exhibited a smaller color difference and water sorption value than composite resin and a greater color difference and water sorption value than polyether-ether-ketones. The ΔEs after coffee immersion were significantly correlated with the water sorption value. The ΔE of FRC with fiber orientations perpendicular to the surface was greater than that of FRC with fiber orientations parallel to the surface, likely due to greater exposure of the matrix-fiber interface. This result suggested that the fiber orientations of FRC affected the discoloration.


Subject(s)
Coffee , Composite Resins , Immersion , Ketones , Computer-Aided Design , Water , Materials Testing , Surface Properties , Color
15.
Dent Mater J ; 42(1): 79-85, 2023 Jan 31.
Article in English | MEDLINE | ID: mdl-36351601

ABSTRACT

The purpose of the present study was to evaluate the influence of height and length variations of alumina ceramics manufactured by stereolithography on deformations caused by the manufacturing process and on the 3D shrinkage ratio to control the final dimensions and improve the adaptation of stereolithographic ceramic dental prostheses. Two different U-shaped models were designed with variable heights or lengths. The specimens were manufactured by stereolithography and were scanned using a microtomographic device before and after the heat treatment. Dimensional variations were measured using inspection software. The number and surface of layers of alumina ceramic influenced the reliability of the stereolithography manufacturing but did not influence the 3D shrinkage ratio. The larger the layer surface, the larger the deformation of the ceramic. Dental ceramics manufactured by stereolithography with smallest layer surface are the most reliable. This helps in the selection of the build orientation.


Subject(s)
Aluminum Oxide , Dental Porcelain , Reproducibility of Results , Computer-Aided Design , Ceramics , Materials Testing
16.
J Esthet Restor Dent ; 35(2): 390-396, 2023 Mar.
Article in English | MEDLINE | ID: mdl-36057856

ABSTRACT

OBJECTIVE: To compare the color stability, translucency, and biaxial flexural strength (BFS) of differently glazed advanced lithium disilicate (ALDS) with those of lithium disilicate (LDS) and zirconia-reinforced lithium silicate (ZLS) after coffee thermocycling. MATERIALS AND METHODS: Forty disk-shaped specimens were prepared from three lithium silicate based materials (CEREC Tessera, ALDS; IPS e.max CAD, LDS; Vita Suprinity, ZLS). ALDS specimens were divided into two subgroups according to glazing procedures (reduced glaze duration, ALDS-S and normal glaze duration, ALDS-N), while LDS and ZLS specimens were crystallized and glazed. Color coordinate measurements were performed before and after coffee thermocycling. Color differences (ΔE00 ) and relative translucency parameters (RTP) were calculated. Specimens were then subjected to BFS test. Statistical analysis was performed by using 1- (ΔE00 and BFS) and 2-way (RTP) ANOVA tests (α = 0.05). RESULTS: ΔE00 values of tested materials were similar (df = 3, F = 0.150, p = 0.929). Two-way ANOVA showed the significant effect of material type, coffee thermocycling, and the interaction between these parameters on RTP values (p < 0.001). Both before and after thermocycling, LDS had the highest (p ≤ 0.001) and ZLS had the lowest (p < 0.001) RTP values, while ALDS-N had higher RTP than ALDS-S (p ≤ 0.001). Among tested materials, only LDS had similar RTP values before and after thermocycling (p = 0.865) as the other materials had lower RTP values after thermocycling (p < 0.001). ALDS-N had higher BFS values than ALDS-S (p = 0.005), while LDS had similar values to ALDS specimens (p ≥ 0.201). ZLS had the highest BFS (p ≤ 0.007). CONCLUSIONS: ALDS had comparable values to those of other materials. However, reduced glazing duration resulted in decreased translucency and BFS of ALDS. CLINICAL SIGNIFICANCE: ALDS may be an appropriate restorative material for those patients with increased coffee consumption considering its color stability and ability to maintain translucency, particularly when glazed by using a conventional porcelain furnace.


Subject(s)
Dental Porcelain , Flexural Strength , Humans , Coffee , Lithium , Materials Testing , Color , Computer-Aided Design , Surface Properties , Ceramics , Silicates , Zirconium
17.
Int J Mol Sci ; 23(9)2022 Apr 25.
Article in English | MEDLINE | ID: mdl-35563129

ABSTRACT

Influenza A is an acute respiratory infectious disease caused by the influenza A virus, which seriously threatens global human health and causes substantial economic losses every year. With the emergence of new viral strains, anti-influenza drugs remain the most effective treatment for influenza A. Research on traditional, innovative small-molecule drugs faces many challenges, while computer-aided drug design (CADD) offers opportunities for the rapid and effective development of innovative drugs. This literature review describes the general process of CADD, the viral proteins that play an essential role in the life cycle of the influenza A virus and can be used as therapeutic targets for anti-influenza drugs, and examples of drug screening of viral target proteins by applying the CADD approach. Finally, the main limitations of current CADD strategies in anti-influenza drug discovery and the field's future directions are discussed.


Subject(s)
Influenza A virus , Influenza, Human , Antiviral Agents/pharmacology , Antiviral Agents/therapeutic use , Computer-Aided Design , Drug Design , Drug Discovery , Drug Evaluation, Preclinical , Humans , Influenza, Human/drug therapy
18.
BMC Oral Health ; 22(1): 180, 2022 05 14.
Article in English | MEDLINE | ID: mdl-35568863

ABSTRACT

BACKGROUND: The aim of this study is to evaluate the color stability of hybrid ceramics stored in different combinations of beverages that are routinely consumed. METHODS: The specimens were prepared with resin nano-ceramic (Lava Ultimate, 3M Espe, USA) and hybrid ceramic (Vita Enamic, Vita Zahnfabrik, Germany). The specimens were aged in a thermocycler machine for 10,000 cycles. They were stored in different combinations of beverages (water, tea, coke, coffee, red wine, pomegranate juice, and turnip juice) for 12 + 12 h. Surface roughness measurements were performed using a profilometer. The specimen colors were measured using a spectrophotometer. The color values (L-a-b) of the specimens and mean surface roughness values (Ra) were recorded at the end of the 1st (D1), 7th (D7), 14th (D14) and 28th (D28) d. RESULTS: When the solution groups were examined, significant color changes were observed in the Lava coffee-tea, Enamic coffee-tea, Lava coffee-wine, and Enamic coffee-wine groups compared with the other groups (p < 0.01). Except for the samples in the Lava coffee-wine 28th day (D28) and Enamic coffee-wine 28th day (D28) groups, more color changes were observed in the Lava samples than in the Enamic samples across all groups and periods. CONCLUSION: Greater color changes (except for the samples stored in coffee-wine) were observed in the Lava samples than in the Enamic samples across all groups and periods. It was observed that the coffee-tea and coffee-wine beverage combinations produced the greatest color change in hybrid ceramics within the limitations of this study.


Subject(s)
Coffee , Composite Resins , Aged , Beverages , Ceramics , Color , Computer-Aided Design , Humans , Materials Testing , Surface Properties , Tea
19.
J Prosthet Dent ; 127(4): 659.e1-659.e11, 2022 Apr.
Article in English | MEDLINE | ID: mdl-35184887

ABSTRACT

STATEMENT OF PROBLEM: Studies on the behavior of computer-aided design and computer-aided manufacturing (CAD-CAM) monolithic materials subjected to gastric juice alternating with brushing-as occurs in patients with bulimia nervosa-are lacking. PURPOSE: The purpose of this in vitro study was to evaluate, over a simulated 5-year period, the effect of gastric juice alternating with brushing on the roughness, topography, and staining susceptibility of CAD-CAM monolithic materials. MATERIAL AND METHODS: Disks of Lava Ultimate (LU), Vita Enamic (VE), IPS Empress CAD (EMP), IPS e.max CAD (EMAX), and Vita Suprinity (VS) were randomly allocated to artificial saliva+brushing or gastric juice+brushing groups, simulating 1, 3, and 5 years of clinical function. The roughness (Sa) and topography were evaluated at baseline (T0) and at each simulated year. For the staining susceptibility (ΔE00), the CIELab color coordinates were registered at baseline, and, at the end of the fifth simulated year, the specimens were immersed in deionized water, coffee, or cola before the second reading. Roughness data were submitted to mixed repeated-measures ANOVA and Bonferroni, and the staining susceptibility data were analyzed by 3-way ANOVA and the Games-Howell test (α=.05). RESULTS: The gastric juice+brushing led to higher roughness than artificial saliva+brushing only in the VE at T3 and T5 (P<.01). In both treatments, the LU and VE showed topography changes and an increase in roughness over time (P<.001), in addition to higher roughness than the other materials (P<.001). The staining susceptibility of the materials to each staining solution was not affected by the treatment (P>.05). The LU and VS groups were more stained by coffee (P<.001), while the VE and EMP groups were more stained by cola (P≤.016), except for the EMP in the gastric juice+brushing, where no significant difference was found between cola and coffee (P>.05). The EMAX was imperceptibly affected by the 3 solutions. CONCLUSIONS: Concerning roughness and topography, the LU and VE were the most affected by both treatments. The staining susceptibility of the materials was not affected by the treatment.


Subject(s)
Coffee , Dental Porcelain , Ceramics , Color , Computer-Aided Design , Gastric Juice , Humans , Materials Testing , Saliva, Artificial , Staining and Labeling , Surface Properties
20.
Pesqui. bras. odontopediatria clín. integr ; 22: e220098, 2022. tab, graf
Article in English | LILACS, BBO | ID: biblio-1422252

ABSTRACT

Abstract Objective: To evaluate the impact of the originally-developed approach aimed at pre-treatment graphical modelling of soft-tissue changes (digital soft tissue design) for the optimization of patient-centered outcomes after Class I and Class II single gingival recessions treatment with the use of a xenogeneic dermal matrix. Material and Methods: Patients enrolled in the study group received single gingival recession treatment via CAF+XDM method supported by pre-treatment graphical modelling of potential soft-tissue changes (digital soft tissue design), while patients enrolled in the control group received single gingival recession treatment via CAF+CTG method with no pre-treatment graphical modeling of gingival level changes. Patient-centered outcomes were measured by visual analogue scale, OHIP-14, and Mahajan's scales. Results: Realization of pre-treatment graphical modelling of soft-tissue changes supported the achievement of better patient-centered outcomes, such as root coverage (p<0.05), surgical phase (p<0.05), post-surgical phase (p<0.05), cost-effectiveness (p<0.05) and diagnostics and patient-orientation (p<0.05) based on patient's personal perception grades. Conclusion: Patient-centered results were found to be more successful within the group using the xenogeneic type of graft accompanied with the implementation of pre-treatment graphical modeling of soft tissue changes, which helped to balance patients' pre-operative expectations and post-operative satisfaction with the received results, reduce post-operative morbidity and improve oral health-related quality of life (AU).


Subject(s)
Humans , Male , Female , Quality of Life , Treatment Outcome , Therapy, Soft Tissue/methods , Gingival Recession/surgery , Computer-Aided Design , Statistics, Nonparametric